MISCO HN-2 is a nickel base heat resisting casting alloy recommended for services up to 2050 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-42. Producer or source: Michigan-Standard Alloy Castings Company.