UDIMET is a nickel base alloy recommended for applications where high strength at elevated temperatures is required. This datasheet provides information on composition and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-28. Producer or source: Special Metals Inc.. Originally published October 1956, revised December 1961.