Abstract

Molybdenum-rhenium alloy is available in wire, tubing, and sheet products for the electronics, nuclear, and space industries. This datasheet provides information on composition and physical properties. It also includes information on heat treating. Filing Code: MO-17. Producer or source: Rhenium Metals Inc. (Rhenium Alloys Inc.). Originally published January 1999, corrected April 1999.