Abstract

TZM is a molybdenum-base alloy having good formability and good high temperature properties. It is recommended for structural parts operating at very high temperature levels, as well as for tools such as extrusion dies and die casting cores. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Mo-5. Producer or source: Climax Molybdenum Company of Michigan Inc..