Abstract

Climelt Molybdenum-30% W was designed mainly for ultra-high temperature service where a higher melting point than molybdenum metal is needed. It has also found applications in handling molten zinc because of its high corrosion resistance to this corrosive medium. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Mo-4. Producer or source: Climax Molybdenum Company of Michigan Inc..