Abstract

Magnesium AM50A is a die casting alloy and has good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Mg-87. Producer or source: Multiple producers.