Abstract

ELEKTRON AZM is a magnesium extrusion alloy having a high strength level. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Mg-45. Producer or source: Magnesium Elektron Ltd.