Abstract

MAGNESIUM EK30A is a rare-earth type magnesium sand casting alloy recommended for applications requiring good creep properties at 300 to 500 F. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Mg-35. Producer or source: Magnesium foundries.