Abstract
ELECTRON Z5Z is a heavy duty magnesium alloy for structural purposes at normal temperatures. It is characterized by high yield strength with good elongation, high fatigue strength with very low notch sensilivity, and uniform strength in varying sections. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Mg-5. Producer or source: Aluminum Laboratories Ltd. Originally published April 1953, revised June 1959.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Corrosion-resistant alloys
Cast magnesium alloys
Magnesium alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Workability
Compressive strength
Elastic modulus
Fatigue properties
Fracture toughness
Hardness
Tensile properties
Elongation
Physical properties
Thermal properties