Abstract

Carpenter Low Expansion 39 alloy is a 39% nickel iron alloy with a low rate of thermal expansion useful to temperature ranges up to 316 deg C (600 deg F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: FE-132. Producer or source: Carpenter Technology Corporation.