Abstract

NK Super BR-Core is a soft magnetic material that has low residual induction and low core losses at high frequencies compared with conventional silicon steel sheet. In addition, NK Super Br-Core has high saturation induction. This datasheet provides information on composition and physical properties. Filing Code: FE-121. Producer or source: NKK Corporation, Keihin Works.