These alloys are all in the nickel-iron alloy system and are designed with expansion rates closely matching those of certain ceramic materials, including glasses. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. Filing Code: FE-120. Producer or source: AMETEK Specialty Metal Products.