Abstract

PYROMET ALLOY CTX-909 exhibits a low and relatively constant thermal coefficient of expansion over a broad temperature range, high hot hardness and good thermal fatigue resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-89. Producer or source: Carpenter.