METGLAS Alloy 2605SC is an amorphous iron-base, general-purpose, soft magnetic alloy with properties superior to conventional crystalline electrical steels. It offers a unique combination of high resistivity, high saturation induction and extremely low core loss; these characteristics make it suitable for use from low frequencies to very high frequencies. Its applications include transformers and other devices requiring a square-loop high-saturation material. This datasheet provides information on composition and physical properties. It also includes information on forming and heat treating. Filing Code: Fe-64. Producer or source: Allied Corporation, Metglass Products Department.