Abstract

TECHALLOY GLASSEAL 42 is an iron-nickel alloy with thermal expansion that closely matches the 1075 glass. Also, it is sometimes used for sealing action for the 0120 and 0010 glasses. It has the lowest expansivity of the iron-nickel alloys that are commonly used for glass-sealing applications. It is made under strict metallurgical control to provide uniformity of performance. Among its uses are sealed-beam automobile headlamps, ceramic-to-glass seals and industrial lamps. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-59. Producer or source: Techalloy Company Inc..