PYROTOOL A has been designed to display high strength and good ductility at temperatures up to 1200 F. It is used for high-temperature tooling, extrusion dies, liners, dummy blocks, forging dies, mandrels, holders, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-47. Producer or source: Carpenter.