Abstract

CERAMVAR is an iron, nickel, cobalt alloy specially designed and suited for ceramic-to-metal sealing. It has expansion characteristics closely matching those of high temperature alumina ceramics. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, machining, joining, and surface treatment. Filing Code: Fe-21. Producer or source: Wilbur B. Driver Company.