Abstract

Wieland-G07 is a cast high leaded tin bronze subject to medium stress in slide bearing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on low temperature performance as well as heat treating and joining. Filing Code: Cu-869. Producer or source: Wieland Metals Inc..