Abstract

Trojan is a high-strength precipitation hardening copper-nickel-silicon alloy. It also has industrial media for safety in engineering. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well as forming and joining. Filing Code: Cu-847. Producer or source: Columbia Metals Ltd.

This content is only available as a PDF.
You do not currently have access to this content.