Abstract

BrushForm 65 is designed for both superior performance and high reliability in appliance, automotive, and computer power applications. Alloy BF-65’s combination of properties limits power loss at the contact interface, controls temperature rise from resistive heating, and provides stable contact force at temperatures to 200 C (390 F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on forming. Filing Code: Cu-821. Producer or source: Materion Brush Performance Alloys.