Abstract

Ansonia alloys C27000 and C27200 are yellow in color and sufficiently similar to those properties of C26000 to make them interchangeable. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-807. Producer or source: Ansonia Copper & Brass Inc..