Ansonia alloy ACB Hitenso C16200 is a cadmium-containing copper alloy used to increase tensile strength while maintaining electrical conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-805. Producer or source: Ansonia Copper & Brass Inc..