PCLW-SNX alloy is a copper-base negative extension wire used instead of platinum as a compensating leg in Type S and R thermocouples. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-803. Producer or source: Carpenter Technology Corporation.