ELECTRALLOY EC63000 and EC63200 are age-hardenable nickel-aluminum-bronze alloys with strength and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-776. Producer or source: Electralloy, a Division of G.O. Carlson Inc.