Ansonia alloy C24000 is a 20% Zn alloy with the trade name of low brass. It is often used in musical instruments and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-774. Producer or source: Ansonia Copper & Brass Inc.