Abstract

Luvata C425 is a copper alloy with good spring properties and good electrical and thermal conductivity used in electrical contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-764. Producer or source: Luvata Sales (USA) Inc.