Brush Wellman Q-Max tube is a high-strength age-hardening copper alloy with excellent biological resistance for use in waters as condenser tubing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-739. Producer or source: Brush Wellman Inc.