Abstract

OF-OK, oxygen-free copper, has one of the highest thermal and electrical conductivities among the copper grades. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on forming, heat treating, and joining. Filing Code: CU-734. Producer or source: Outokumpu Copper (USA) Inc.