Wieland-M20 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn products such as lipstick cases. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-711. Producer or source: Wieland Metals Inc., Wieland-Werke AG.