Abstract

Wieland-S40 has very high wear resistance. The alloy is used in hot stamped parts requiring high mechanical strength and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion and wear resistance as well as forming, heat treating, and joining. Filing Code: CU-701. Producer or source: Wieland Metals Inc., Wieland-Werke AG.