Abstract

Wieland Z31 is a medium-leaded grade with a good machining of the drop-forged part. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: CU-680. Producer or source: Wieland Metals Inc., Wieland-Werke AG.

This content is only available as a PDF.