Abstract

Brushform 290 is a high-strength beryllium-copper alloy used in electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming. Filing Code: CU-650. Producer or source: Brush Wellman Inc. See also Alloy Digest Cu-505, January 1986.