Abstract

Olin C195 is a high-strength, high-conductivity copper alloy developed for applications in current-carrying parts. Typical applications are electrical springs, connectors, and clips. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-649. Producer or source: Olin Brass.