Abstract

WRM alloy 4222 is a copper-zinc alloy of the tin-brass family with a good combination of conductivity, strength, and forming characteristics. A typical application is in high-performance conductive springs. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-639. Producer or source: Waterbury Rolling Mills Inc.