Abstract

WRM alloy 5118 is a modified phosphor bronze alloy that exhibits improved strength while maintaining good stress-relaxation characteristics. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CU-636. Producer or source: Waterbury Rolling Mills Inc. Originally published June 1999, corrected October 1999.

This content is only available as a PDF.
You do not currently have access to this content.