WRM Alloy 5075 is a modified phosphor bronze with an electrical conductivity and tensile combination superior to those of standard phosphor bronzes. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming. Filing Code: CU-629. Producer or source: Waterbury Rolling Mills Inc. Originally published February 1999, corrected October 1999, revised August 2000.