Abstract

WRM alloy 4252 is a modified copper-zinc-tin alloy similar to C42500 (see Alloy Digest Cu-280, June 1974), with improved conductivity, strength, and forming properties. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CU-619. Producer or source: Waterbury Rolling Mills Inc.