AMPCO-TRODE 150 is recommended for overlay application and welding AMPCO 18 alloy (Alloy Digest Cu-51, June 1957). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-585. Producer or source: Ampco Metal Inc.