BRUSH chromium copper alloys are heat treatable, corrosion resistant alloys with both high electrical conductivity and strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and machining. Filing Code: Cu-579. Producer or source: Brush Wellman Inc..