BRUSH 1915 is a heat-treatable leaded copper alloy engineered for automatic screw machining applications when high strength is needed. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on heat treating and machining. Filing Code: Cu-572. Producer or source: Brush Wellman Inc..