Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553. Producer or source: Copper and copper alloy mills.