COPPER ALLOY No. C36000 is a free cutting brass that is widely used in components and systems-products controlling motion, flow and pressure. High productivity, extended cutting tool life and good corrosion resistance are among its assets. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-548. Producer or source: Brass mills.