Copper Alloy No. C92800 is a cast bronze containing nominally 16% tin and 5% lead. Former commercial names (not recommended) are (1) 295, (2) Leaded Tin Bronze, (3) Ring Metal and (4) 79-16-5-0. It has excellent machinability, moderate strength and good resistance to corrosion. A typical use is piston rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-490. Producer or source: Copper alloy foundries.