Abstract

MUELLER Alloy 6733 is a low-leaded bearing alloy designed for use where ductility and cold working are necessary for such operations as spinning or forming. It can be used with hard or soft mating members. This alloy can be joined by soft or silver soldering. Among the many applications for Mueller Alloy 6733 are clutch bearings, cams, pump gears and seal rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-484. Producer or source: Mueller Brass Company.