MUELLER Alloy 2700 is a medium-strength copper-zinc (brass) alloy with good ductility. It has good resistance to corrosion and excellent cold-working characteristics. It can be cold worked by the conventional fabrication processes. Its many applications include products made from wire for automotive, electrical, architectural and hardware uses. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-456. Producer or source: Mueller Brass Company.