Abstract

Copper Alloy No. C51100 is a copper-tin-phosphorus alloy with relatively high tensile and yield strengths, good ductility and good resistance to corrosion. It can be fabricated by a number of conventional processes. Its many applications include bridge bearing plates, numerous hardware uses such as bellows, clutch disks, fasteners, springs and textile machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-412. Producer or source: Copper and copper alloy mills.