ANACONDA Alloy 210 has a composition that imparts to it a slightly greater strength than copper, corrosion resistance about the same as copper, and an excellent resistance to stress-corrosion cracking. It has good hot-working properties and excellent cold-working characteristics. Among its many applications are coinage, munitions, novelties and a wide range of miscellaneous uses. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-406. Producer or source: Anaconda American Brass Company.