Abstract

Copper Alloy No. C95800 is a copper-aluminum-nickel-iron-manganese alloy with high strength and hardness. It also is characterized by excellent resistance to corrosion and good resistance to fatigue and wear. It is suited for service up to 750 F. Typical uses comprise hubs and blades of ship propellers and other components for contact with salt water. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-397. Producer or source: Copper alloy foundries.