Abstract

ANACONDA (A) 5090, long a specialty item in the industry, is a wrought intermediate phospor bronze developed to fulfill a need for special end-products such as kettles and other containers. It has found broad applications in the chemical industry. It offers a good combination of strength, ductility, resilience, fatigue properties and resistance to both corrosion and erosion. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-372. Producer or source: Anaconda American Brass Company.