Abstract

Copper Alloy No. 844 is a free-cutting copper-tin-lead-zinc alloy for castings; it was formerly identified as 81-3-7-9 alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. It is used widely for fittings, plumbing goods and valves. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-349. Producer or source: Copper alloy foundries.

This content is only available as a PDF.
You do not currently have access to this content.